二碲化鎢晶體 WTe2(Tungsten Diluride) 晶體尺寸:10毫米電學(xué)性能:半金屬,type II Weyl semimetal (WSM)晶體結(jié)構(gòu):斜方晶系 P晶胞參數(shù):a = 0.348 nm, b = 0.625 nm, c = 1.405 nm, α = β = γ = 90#176;晶體類型:合成晶體純度:>99.995%屬性:半導(dǎo)體
二碲化鎢晶體 WTe2(Tungsten Diluride)
晶體尺寸:10毫米
電學(xué)性能:半金屬,type II Weyl semimetal (WSM)
晶體結(jié)構(gòu):斜方晶系 P
晶胞參數(shù):a = 0.348 nm, b = 0.625 nm, c = 1.405 nm, α = β = γ = 90°
晶體類型:合成
晶體純度:>99.995%
屬性:半導(dǎo)體
![](https://img79.86175.com/d4728b83567c7315392130b29f5319771ed744849f5a8f4a8cc624dfbe2a5a4442fcafd6913e1833.jpg)
X-ray diffraction on a WTe2 single crystal aligned along the (001) plane. XRD was performed at room temperature using a D8 Venture Bruker. The 5 XRD peaks correspond, from left to right, to (00l) with l = 2, 4, 6, 8, 10
![](https://img79.86175.com/d4728b83567c7315392130b29f531977fb6806fb96ed32c54254ea93d2886864544fe09296e28b38.jpg)
Powder X-ray diffraction (XRD) of a single crystal WTe2. X-ray diffraction was performed at room temperature using a D8 Venture Bruker.
![](https://img79.86175.com/d4728b83567c7315392130b29f531977e5691aa64c71673e64b6f223962ce116f6f2fe744bfc12d8.jpg)
Stoichiometric analysis of a single crystal WTe2 by Energy-dispersive X-ray spectroscopy (EDX).
![](https://img79.86175.com/d4728b83567c7315392130b29f53197769dc4df9ebc2f2e4cdfb138080240a2f2c2790633ea33394.jpg)
Raman spectrum of a single crystal WTe2. Measurement was performed with a 785 nm Raman system at room temperature.